Since its discovery in 2004, graphene has inspired researchers around the world as the material of the future. In this talk, we will provide an overview of the unique material properties of graphene and discuss the material synthesis and device processing technology developed here at MIT for large area applications. Finally, leveraging the unique carrier transport properties of graphene, we present some preliminary results on graphene-based thermopiles for infrared imaging applications.